| PROBLEM |
LOOK FOR |
| Low Gloss |
High humidity, dirty mop, poor rinsing of the cleaning chemicals, recoated too soon, material was frozen.
|
| Scuffing |
Coats are too heavy |
| Powdering |
Low humidity, freshly stripped floor, pooly sealed, allowed to become "bone dry" before coating, drafts promoting fast vaporization of the film, coats too thin.
|
| Streaking |
Dirty floor, dirty mop, pronounced high humidity recoated too soon.
|
| Fish Eyes |
Greasy floor, soap film.
|
| Peeling, no adhesion |
This can mistakenly be judged as extreme case of powdering. Some old waxy floor finish underneath new floor with original factory coating.
|
| Black Heel Marks |
Coats are too heavy.
|
| Poor Flow |
Greasy surface. Examine container of the finish used. It was perhaps partly full, stored in a hot area, or not properly closed.
|
|
|